Phosphate and Borate-Based Composite Interface of Single-Crystal LiNi0.8Co0.1Mn0.1O2 Enables Excellent Electrochemical Stability at High Operation Voltage.


ABSTRACT: The application of nickel-rich cathodes in lithium-ion batteries has been hampered by its rapid capacity/voltage fading and limited performance of rate. In this work, a passivation technique is used to create a stable composite interface on single-crystal LiNi0.8Co0.1Mn0.1O2 (NCM811) surface, which greatly improves the cycle life-span and high-voltage constancy of cathode with 4.5 and 4.6 V cut-off voltage. The improved Li+ conductivity of the interface enables a firm cathode-electrolyte interphase (CEI), which reduces interfacial side reactions, lowers the risk of safety hazards, and improves irreversible phase transitions. As a result, the electrochemical performance of single-crystal Ni-rich cathode are remarkably enhanced. The specific capacity of 152 mAh g-1 can be delivered at a charging/discharging rate of 5 C under 4.5 V cut-off voltage, much higher than 115 mAh g-1 of the pristine NCM811. After 200 cycles at 1 C, the composite interface modified NCM811 demonstrates outstanding capacity retention of 85.4% and 83.8% at 4.5 V and 4.6 V cut-off voltage, respectively.

SUBMITTER: Long F 

PROVIDER: S-EPMC10224527 | biostudies-literature | 2023 May

REPOSITORIES: biostudies-literature

altmetric image

Publications

Phosphate and Borate-Based Composite Interface of Single-Crystal LiNi<sub>0.8</sub>Co<sub>0.1</sub>Mn<sub>0.1</sub>O<sub>2</sub> Enables Excellent Electrochemical Stability at High Operation Voltage.

Long Fu F   Liu Yuyang Y   Zhu Guobin G   Wang Yan Y   Zheng Honghe H  

Materials (Basel, Switzerland) 20230509 10


The application of nickel-rich cathodes in lithium-ion batteries has been hampered by its rapid capacity/voltage fading and limited performance of rate. In this work, a passivation technique is used to create a stable composite interface on single-crystal LiNi<sub>0.8</sub>Co<sub>0.1</sub>Mn<sub>0.1</sub>O<sub>2</sub> (NCM811) surface, which greatly improves the cycle life-span and high-voltage constancy of cathode with 4.5 and 4.6 V cut-off voltage. The improved Li<sup>+</sup> conductivity of t  ...[more]

Similar Datasets

| S-EPMC11344168 | biostudies-literature
| S-EPMC10221140 | biostudies-literature
| S-EPMC5206713 | biostudies-literature
| S-EPMC9082506 | biostudies-literature
| S-EPMC11303531 | biostudies-literature
| S-EPMC9661853 | biostudies-literature
| S-EPMC10664004 | biostudies-literature
| S-EPMC9654857 | biostudies-literature
| S-EPMC7816706 | biostudies-literature
| S-EPMC10979152 | biostudies-literature