Electrochemically induced crystalline-to-amorphization transformation in sodium samarium silicate solid electrolyte for long-lasting sodium metal batteries.


ABSTRACT: Exploiting solid electrolyte (SE) materials with high ionic conductivity, good interfacial compatibility, and conformal contact with electrodes is essential for solid-state sodium metal batteries (SSBs). Here we report a crystalline Na5SmSi4O12 SE which features high room-temperature ionic conductivity of 2.9 × 10-3 S cm-1 and a low activation energy of 0.15 eV. All-solid-state symmetric cell with Na5SmSi4O12 delivers excellent cycling life over 800 h at 0.15 mA h cm-2 and a high critical current density of 1.4 mA cm-2. Such excellent electrochemical performance is attributed to an electrochemically induced in-situ crystalline-to-amorphous (CTA) transformation propagating from the interface to the bulk during repeated deposition and stripping of sodium, which leads to faster ionic transport and superior interfacial properties. Impressively, the Na|Na5SmSi4O12|Na3V2(PO4)3 sodium metal batteries achieve a remarkable cycling performance over 4000 cycles (6 months) with no capacity loss. These results not only identify Na5SmSi4O12 as a promising SE but also emphasize the potential of the CTA transition as a promising mechanism towards long-lasting SSBs.

SUBMITTER: Sun G 

PROVIDER: S-EPMC10579357 | biostudies-literature | 2023 Oct

REPOSITORIES: biostudies-literature

altmetric image

Publications

Electrochemically induced crystalline-to-amorphization transformation in sodium samarium silicate solid electrolyte for long-lasting sodium metal batteries.

Sun Ge G   Lou Chenjie C   Yi Boqian B   Jia Wanqing W   Wei Zhixuan Z   Yao Shiyu S   Lu Ziheng Z   Chen Gang G   Shen Zexiang Z   Tang Mingxue M   Du Fei F  

Nature communications 20231016 1


Exploiting solid electrolyte (SE) materials with high ionic conductivity, good interfacial compatibility, and conformal contact with electrodes is essential for solid-state sodium metal batteries (SSBs). Here we report a crystalline Na<sub>5</sub>SmSi<sub>4</sub>O<sub>12</sub> SE which features high room-temperature ionic conductivity of 2.9 × 10<sup>-3</sup> S cm<sup>-1</sup> and a low activation energy of 0.15 eV. All-solid-state symmetric cell with Na<sub>5</sub>SmSi<sub>4</sub>O<sub>12</sub>  ...[more]

Similar Datasets

| S-EPMC9126868 | biostudies-literature
| S-EPMC8953603 | biostudies-literature
| S-EPMC9401571 | biostudies-literature
| S-EPMC6279964 | biostudies-literature
| S-EPMC11489388 | biostudies-literature
| S-EPMC8836821 | biostudies-literature
| S-EPMC9614718 | biostudies-literature
| S-EPMC11320443 | biostudies-literature
| S-EPMC7986800 | biostudies-literature
| S-EPMC10275921 | biostudies-literature