Suppressing Manganese Dissolution via Exposing Stable {111} Facets for High-Performance Lithium-Ion Oxide Cathode.


ABSTRACT: Spinel-type LiMn2O4 cathode materials commonly suffer from manganese dissolution due to the severe interfacial side reactions especially at elevated temperature. Here, a 3D hollow fusiform LiMn2O4 cathode material is reported with preferentially exposed stable {111} facets and seamless outer structure, which is clearly confirmed by microfocused ion beam scanning electron microscopy, high-resolution transmission electron microscopy as well as scanning transmission electron microscopy with atomic resolution. Owing to the optimal geometrical structure design and the preferentially exposed stable {111} facets, the electrode delivers excellent rate capability (107.6 mAh g-1 at 10 C), remarkable cycling stability (83.3% capacity retention after 1000 cycles at 1 C), and outstanding high-temperature performance. Together with the analyses of electrochemical behaviors, in situ X-ray diffraction at different temperatures, and ex situ X-ray photoelectron spectra, the underlying working mechanism for suppressing manganese dissolution is clearly articulated. These findings could provide significant guidelines for precisely designing highly stable cathode materials for LIBs.

SUBMITTER: Xiao Y 

PROVIDER: S-EPMC6662411 | biostudies-literature | 2019 Jul

REPOSITORIES: biostudies-literature

altmetric image

Publications

Suppressing Manganese Dissolution via Exposing Stable {111} Facets for High-Performance Lithium-Ion Oxide Cathode.

Xiao Yao Y   Zhang Xu-Dong XD   Zhu Yan-Fang YF   Wang Peng-Fei PF   Yin Ya-Xia YX   Yang Xinan X   Shi Ji-Lei JL   Liu Jian J   Li Hongliang H   Guo Xiao-Dong XD   Zhong Ben-He BH   Guo Yu-Guo YG  

Advanced science (Weinheim, Baden-Wurttemberg, Germany) 20190429 13


Spinel-type LiMn<sub>2</sub>O<sub>4</sub> cathode materials commonly suffer from manganese dissolution due to the severe interfacial side reactions especially at elevated temperature. Here, a 3D hollow fusiform LiMn<sub>2</sub>O<sub>4</sub> cathode material is reported with preferentially exposed stable {111} facets and seamless outer structure, which is clearly confirmed by microfocused ion beam scanning electron microscopy, high-resolution transmission electron microscopy as well as scanning t  ...[more]

Similar Datasets

| S-EPMC6797712 | biostudies-literature
| S-EPMC8493547 | biostudies-literature
| S-EPMC6456622 | biostudies-literature
| S-EPMC9417273 | biostudies-literature
| S-EPMC6105723 | biostudies-literature
| S-EPMC6797695 | biostudies-literature
| S-EPMC5133657 | biostudies-literature
| S-EPMC9300204 | biostudies-literature
| S-EPMC8457143 | biostudies-literature
| S-EPMC8461773 | biostudies-literature