Gamma irradiation influence on mechanical, thermal and conductivity properties of hybrid carbon nanotubes/montmorillonite nanocomposites.


ABSTRACT: A thermoplastic elastomer (TPE) based nanocomposite with the same weight ratio of hybrid nanofillers composed of carbon nanotubes (CNTs) and montmorillonite nanoclay (DK4) was prepared using a melt blending technique with an internal mixer. The TPE composite was blended from polylactic acid (PLA), liquid natural rubber (LNR) as a compatibilizer and natural rubber (NR) in a volume ratio of 70:10:20, respectively. The weight ratio of CNTs and DK4 was 2.5 wt%. The prepared samples were exposed to gamma radiation at range of 0-250 kGy. After exposure to gamma radiation, the mechanical, thermo-mechanical, thermal and electrical conductivity properties of the composites were significantly higher than unirradiated TPE composites as the irradiation doses increased up to 150 kGy. Transmission electron microscopy (TEM) micrographs revealed the good distribution and interaction between the nano-fillers and the matrix in the prepared TPE hybrid nanocomposites. In summary, the findings from this work definite that gamma irradiation might be a viable treatment to improve the properties of TPE nanocomposite for electronic packaging applications.

SUBMITTER: Tarawneh MA 

PROVIDER: S-EPMC7568474 | biostudies-literature | 2021 Feb

REPOSITORIES: biostudies-literature

altmetric image

Publications

Gamma irradiation influence on mechanical, thermal and conductivity properties of hybrid carbon nanotubes/montmorillonite nanocomposites.

Tarawneh Mou'ad A MA   Saraireh Sherin A SA   Chen Ruey Shan RS   Ahmad Sahrim Hj SH   Al-Tarawni Musab A M MAM   Yu Lih Jiun LJ  

Radiation physics and chemistry (Oxford, England : 1993) 20201017


A thermoplastic elastomer (TPE) based nanocomposite with the same weight ratio of hybrid nanofillers composed of carbon nanotubes (CNTs) and montmorillonite nanoclay (DK4) was prepared using a melt blending technique with an internal mixer. The TPE composite was blended from polylactic acid (PLA), liquid natural rubber (LNR) as a compatibilizer and natural rubber (NR) in a volume ratio of 70:10:20, respectively. The weight ratio of CNTs and DK4 was 2.5 wt%. The prepared samples were exposed to g  ...[more]

Similar Datasets

| S-EPMC7040804 | biostudies-literature
| S-EPMC10647783 | biostudies-literature
| S-EPMC11327554 | biostudies-literature
| S-EPMC8347775 | biostudies-literature
| S-EPMC7077723 | biostudies-literature
| S-EPMC5353756 | biostudies-literature
| S-EPMC9919012 | biostudies-literature
| S-EPMC9585649 | biostudies-literature
| S-EPMC7825608 | biostudies-literature
| S-EPMC6572346 | biostudies-literature