Mapping the Galvanic Corrosion of Three Metals Coupled with a Wire Beam Electrode: The Influence of Temperature and Relative Geometrical Position.


ABSTRACT: The local electrochemical properties of galvanic corrosion for three coupled metals in a desalination plant were investigated with three wire-beam electrodes as wire sensors: aluminum brass (HAl77-2), titanium (TA2), and 316L stainless steel (316L SS). These electrodes were used with artificial seawater at different temperatures. The potential and current-density distributions of the three-metal coupled system are inhomogeneous. The HAl77-2 wire anodes were corroded in the three-metal coupled system. The TA2 wires acted as cathodes and were protected; the 316L SS wires acted as secondary cathodes. The temperature and electrode arrangement have important effects on the galvanic corrosion of the three-metal coupled system. The corrosion current of the HAl77-2 increased with temperature indicating enhanced anode corrosion at higher temperature. In addition, the corrosion of HAl77-2 was more significant when the HAl77-2 wires were located in the middle of the coupled system than with the other two metal arrangement styles.

SUBMITTER: Ju H 

PROVIDER: S-EPMC5872936 | biostudies-literature | 2018 Feb

REPOSITORIES: biostudies-literature

altmetric image

Publications

Mapping the Galvanic Corrosion of Three Metals Coupled with a Wire Beam Electrode: The Influence of Temperature and Relative Geometrical Position.

Ju Hong H   Yang Yuan-Feng YF   Liu Yun-Fei YF   Liu Shu-Fa SF   Duan Jin-Zhuo JZ   Li Yan Y  

Materials (Basel, Switzerland) 20180228 3


The local electrochemical properties of galvanic corrosion for three coupled metals in a desalination plant were investigated with three wire-beam electrodes as wire sensors: aluminum brass (HAl77-2), titanium (TA2), and 316L stainless steel (316L SS). These electrodes were used with artificial seawater at different temperatures. The potential and current-density distributions of the three-metal coupled system are inhomogeneous. The HAl77-2 wire anodes were corroded in the three-metal coupled sy  ...[more]

Similar Datasets

| S-EPMC5951518 | biostudies-literature
| S-EPMC9946947 | biostudies-literature
| S-EPMC7192930 | biostudies-literature
| S-EPMC5490352 | biostudies-other
| S-EPMC6363004 | biostudies-literature
| S-EPMC10706957 | biostudies-literature
| S-EPMC4510135 | biostudies-literature
| S-EPMC9897567 | biostudies-literature
| S-EPMC5865079 | biostudies-literature
| S-EPMC8551296 | biostudies-literature