Achievement of Room Temperature Superelasticity in Ti-Mo-Al Alloy System via Manipulation of ω Phase Stability.


ABSTRACT: The achievement of room-temperature (RT) superelasticity in a Ti-Mo-Al ternary alloy system through the addition of a relatively high concentration of Al to manipulate the phase stability of the ω phase is realized in this study. The composition of the Ti-6 mol% Mo (Ti-11.34 mass% Mo) alloy was designated as the starting alloy, while 5 mol% Al (=2.71 mass% Al) and 10 mol% Al (=5.54 mass% Al) were introduced to promote their superelastic behavior. Among the alloys, Ti-6 mol% Mo-10 mol% Al alloy, which was investigated for the very first time in this work, performed the best in terms of superelasticity. On the other hand, Ti-6 mol% Mo and Ti-6 mol% Mo-5 mol% Al alloys exhibited a shape memory effect upon heating. It is worth mentioning that in the transmission electron microscopy observation, ω phase, which appeared along with β-parent phase, was significantly suppressed as Al concentration was elevated up to 10 mol%. Therefore, the conventional difficulties of the inhibited RT superelasticity were successfully revealed by regulating the number density of the ω phase below a threshold.

SUBMITTER: Nohira N 

PROVIDER: S-EPMC8836841 | biostudies-literature | 2022 Jan

REPOSITORIES: biostudies-literature

altmetric image

Publications

Achievement of Room Temperature Superelasticity in Ti-Mo-Al Alloy System via Manipulation of ω Phase Stability.

Nohira Naoki N   Chiu Wan-Ting WT   Umise Akira A   Tahara Masaki M   Hosoda Hideki H  

Materials (Basel, Switzerland) 20220123 3


The achievement of room-temperature (RT) superelasticity in a Ti-Mo-Al ternary alloy system through the addition of a relatively high concentration of Al to manipulate the phase stability of the ω phase is realized in this study. The composition of the Ti-6 mol% Mo (Ti-11.34 mass% Mo) alloy was designated as the starting alloy, while 5 mol% Al (=2.71 mass% Al) and 10 mol% Al (=5.54 mass% Al) were introduced to promote their superelastic behavior. Among the alloys, Ti-6 mol% Mo-10 mol% Al alloy,  ...[more]

Similar Datasets

| S-EPMC4643295 | biostudies-literature
| S-EPMC6362253 | biostudies-literature
| S-EPMC5453936 | biostudies-literature
| S-EPMC9972530 | biostudies-literature
| S-EPMC9679436 | biostudies-literature
| S-EPMC5553093 | biostudies-literature
| S-EPMC8400223 | biostudies-literature
| S-EPMC7191259 | biostudies-literature
| S-EPMC10240522 | biostudies-literature
| S-EPMC5988503 | biostudies-literature